HPMC dividi potest in: constructionem gradus, gradus cibi et gradus medicinae secundum usum. Hoc temporeChina is constructione gradus plerumque in aedificando genere;Murus putty/Skim Coat dosisVERRO tunica pulvis magnus valde. Pulvis HPMC et multa alia medicamenta pulverulenta cum mixtura mixta, adde aquam dissolvere, hoc tempore HPMC dissolvere potest, sed non agglomerare, quia unumquodque minutum angulum, paululum HPMC pulveris, aqua statim dissolvet.Skim Coatpulveris et mortarii incepti productionis huiusmodi methodo utuntur. Hydroxypropyl yl cellulosum (HPMC) crassiore et aqua conservante in mortario puttoso adhibetur.

 

Temperatura gel de HPMC ad metoxylum contentum refertur, contentum methoxylum inferioremdeorsumaltior gel temperies up. HPMC aquae frigidae instans solutio speciei post curationem glyoxalis superficiei positae in aqua frigida cito dispergitur, sed non vere dissolvitur, viscositas sursum dissolvitur. Thermosoluble HPMC genus non est superficies glyoxal tractata. Moles glyoxalis magna est, dissipatio celeris, viscositas tarda est, moles e contrario parva est. HPMC dividi potest in instans et calor solubilis, instant producta, cito dispersa in aqua frigida, evanuit in aqua, hoc tempore humor nullam viscositatem habet, quia HPMC in aqua solum dispergitur, nulla est vera dissolutio. Circa 2 minuta, viscositas liquidi paulatim crescit, colloideum viscosum diaphanum efformans. Calor solubilis productorum, in aqua frigida agglomeratio, potest esse in aqua calida, cito dispersa, in aqua calida evanescere, donec temperatura guttae ad aliquam temperiem, viscositas lente apparebit, donec formatio viscosi pellucidis colloidei. Calor solutum genus non potest esse nisi inSkim Coat et luti, in liquida gluten et efficiens, potest videri agglomeratio phaenomenon, uti non potest. Instanti solvendi exemplar, scopo applicatio pauca latius, inSkim CoatPulvis et caementum, et gluten liquidum et efficiens, omnia utantur, quae tabo non habent.

 

Methodus solvendi productionis HPMC, toluene facta, alcohol solvens isopropyl, si lavatio non est valde bona, gustus residua erit. per applicationem deSkim Coat  pulveris: requisitio inferior, viscositas 100000refert, aquam proximam tueri. Mortarium applicatio: requisita superiora, viscositas requisita alta, 150000 meliores esse. Gluten applicatio: opus instantis producti, alta viscositas. HPMC in ipsa applicatione quantitatis, per ambitum climatis, temperiem, localem calcii cinerei qualitatem;Skim Coat formulae et "exiguitatis mos qualitatis" diversorum, ac sunt differentiae. Hydroxypropyl yl cellulosum (HPMC) viscositatis -Skim Coatpulveris is100000quidam altiores in caemento, 150 milia facultatis uti volunt. HpMC autem munus principale est ut aquam retineat, deinde crasso. InSkim CoatSi autem aqua retentione bona est, viscositas est humilis (7-80 .000) potest etiam viscositas maior, et relativa aqua retentione melior, quando viscositas plus quam 100 est.000viscositas aquae retentionis non est multum; Hydroxypropyl contentum altum est, aqua retentio fere melior est. Viscositas, aqua retentio, melius, et viscositas, in caemento caemento melius adhibetur.

 

 

HPMC inSkim Coatcrasso, aqua retentione et constructione trium functionum. Praesent dapibus aliquam elit. Bulla aquae nimium causa sit, imo etiam non siccus, in summitate iacuit radendo, etiam bullire facile. HPMC in crasso effectus estSkim Coat: cellulosa ad suspensionem incrassari potest, ut solutio uniformis sursum et deorsum partes anti-fluentis pendentis remaneat. HPMC aqua retentione effectum inSkim Coat: facereSkim Coat lente excoquatur, auxilium calcium griseum reactionem sub actione aquae. HPMC inSkim Coat constructione munus: cellulosa lubricatio, potest facereSkim Coat habet bonam constructionem. HPMC quaslibet reactiones chemicae non participat, sed tantum munus sustinet.

 

 

Murus putty/Skim Coat pulvis et cinis calcii principalis qualitas magnam relationem habet, et HPMC magnam relationem non habet. Humilis calcii contentum calcii grisei et impropriam proportionem CaO et Ca(OH)2 in calcii griseo faciet pulverem stillantem. Si parum necessitudinis cum HPMC, tunc est retentio aquae pauperis HPMC, etiam pulveris causa;Skim Coat et aqua in muro est reactionis chemica propter generationem substantiarum novarum, pariesSkim Coat de muro, attritum in pulverem, et postea utere, non linea, quia novam substantiam formavit (calcium carbonas). Partes principales cineris calcii grisei sunt: ​​Ca(OH)2, CaO et parva mixtionis copia CaCO3, CaO+H2O=Ca(OH)2 - Ca(OH)2+CO2=CaCO3+H2O calcii grisei in aqua et aere sub actione CO2, formatio carbonis calcii, et HPMC tantum aqua, griseo calcii auxiliaris melioris reactionis est, suam nullam reactionem participavit.

 

Formula omniummurusputty pulveris;

I, parietis interioris ordinarii pulveris putty formulae

Redispersible polymer pulveris RDP 2 ~ 2.2%, pulvisculus muscus duplex (vel talc) 98% HPMC 0.4%

II, murus interioris putty pollinis formulae ordinariae altae durae

Redispersible polymer pulveris RDP 1.8 ~ 2.2%, pulveris muscae duplicis (vel talc pulveris) 90~ 60%, emplastrum Parisiense (aedificatio gypsi, aqua dimidia gypsi) 10 ~ 40% HPMC 0.4%

III, alta duritia et aqua resistentia parietis interioris putty pulveris referendi formula

Formulae I;Redispersible polymer pulveris RDP 1 ~ 1.2%, duplex musca pulveris 70%, calcis calcii pulveris 30% HPMC 0.4%

Formulae duae;Redispersible polymer pulveris RDP 0.8 ~ 1.2%,duplex musca pulveris 60%, cinerei calcii pulveris 20%, caementi albi 20% HPMC 0.4%

4. Alta durities, washable et rubigine probationem parietis interioris putty pulveris referentis formulae

Formulae I;Redispersible polymer pulveris RDP 0.4 ~ 0.45%, duplex musca pulveris 70%, calcii pulveris 30% cinis HPMC 0.4%

Formulae duae;Redispersible polymer pulveris RDP 0.4 ~ 0,45%, duplex musca pulveris 60%, calcii grisei pulveris 20%, caementi albi 20% HPMC 0.4%

5. Relatio de formula altae duritiei, aquae resistentis et fissurae parietis exterioris renitentis pulveris putty

Formulae I;Redispersible polymer pulveris RDP 1.5 ~ 1.9%, caementum album (caementum nigrum) 40%, duplex musca pulveris 30%, calcii grisei pulveris 30%, rima praeventionis additivae 1 ~ 1.5% HPMC 0.4%

 

 

 

Formulae duae;Redispersible polymer pulveris RDP 1.7-1.9%, caementum album (caementum nigrum) 40%, duplex musca pulveris 40%, calcii grisei pulveris 20%, rima praeventionis additivae 1-1.5% HPMC 0.4%

Formulae tres;Redispersible polymer pulveris RDP 2~2.2%, caementum album (caementum nigrum) 40%;duplex musca pulveris 20%, grisei calcii pulveris 20%, vicus pulveris (CLXXX# harenae) 20%, rima praeventionis ELOGIUM 2~3% HPMC 0.4%

Formulae quatuor;Redispersible polymer pulveris RDP 0.6-1%, caementum album (425#) 40%, calcii grisei pulveris 25%, muscae duplex 35%, anti- crepuit additivorum 1.5% HPMC 0.4%

Formulae quinque;Redispersible polymer pulveris RDP 2.5 ~ 2.8%, caementum album (caementum nigrum) 35%, duplex musca pulveris 30%, calcii grisei pulveris 35%, rima praeventionis additivae 1 ~ 1.5% HPMC 0.4%

6

Redispersible polymer pulveris RDP 0,8 ~ 1.8%, caementum album (caementum nigrum) 30%, duplex musca pulveris 40%, calcium cinereum 30%, rima praeventionis additamentum 1 ~ 2% HPMC 0.4%

VII, Mosaic habena tegularum parietis anti-rimam ustam pulveris referat formulam

Formulae I;Redispersible polymer pulveris RDP 1 ~ 1.3%, caementum album (425#) 40%, calcii grisei pulveris 20%, muscae duplex pulvis 20%, anti- crepuit additivus 1.5%, vicus arenae 120 reticulum (vel arena fluminis arida) 20% HPMC 0.4%

Formulae duae;Redispersible polymer pulveris RDP 2.5~3%, caementum album (caementum nigrum) 40%;duplex musca pulveris 20%, grisei calcii pulveris 20%, vicus pulveris (180# arenae) 20%, rima praeventionis additivorum 2~3% HPMC 0.4%

Formulae tres;Redispersible polymer pulveris RDP 2.2 ~ 2.8%, caementum album (caementum nigrum) 40%, duplex musca pulveris 40%, calcii grisei pulveris 20%, rima praeventionis additivae 1 ~ 1.5% HPMC 0.4%

8, Tegula Mosaica elastica parietis exterioris lavabilis anti rima putty pulveris referentis formulae

Redispersible polymer pulveris RDP 1.2 ~ 2.2%, caementum album (caementum nigrum) 30%, duplex musca pulveris 30%, calcii grisei pulveris 20%, vicus pulveris (arenae) 20%, rima praeventionis additivae 2~3% HPMC 0.4%

IX, parietis interioris flexibilis pulveris putty referendi formula

Formulae I;Redispersible polymer pulveris RDP 1.3 ~ 1.5%, duplex musca pulveris 80%, calcii pulveris 20% cinis HPMC 0.4%

Formulae duae;Redispersible polymer pulveris RDP 1.3 ~ 1.5%, duplex musca pulveris 70%, calcii pulveris 20% cinis, caementum album 10% HPMC 0.4%

X, parietis exterioris flexibilis ad putty formulam referentia

Formulae I;Redispersible polymer pulveris RDP 1.5 ~ 1.8%,duplex musca pulveris 55%, calcii grisei pulveris 10%, caementi albi 35%, odii crepentis elogium 0.5% HPMC 0.4%

 

XI, parietis exterioris coloris pulveris putty formula

Color puttyRedispersible polymer pulveris RDP 1-1.5%, caementum album 10%, calcium griseum depuratum (calcium oxydatum70%), 15%, resiliunt praeventionis additamentum 2%, bentonite 5%, vicus arena (albedo85% Pii99%), 15%, luteus Jade pulveris 52%, color putty determinatus 0.2% HPMC 0.4%

XII, tegula tenaces formulae ceramicae

Tegula ceramica tenaces pulveris 1,3% tenaces, caementa communis Portlandiae 48.7%, arena aedificationis (CL~ 30 reticulum) L% HPMC 0.4%

XIII, pulvis arida interface agentis formula

 

 

Arida pulveris interface agenteRedispersible polymer pulveris RDP 1.3%, ordinarium caementum Portland 48,7%, arenam aedificans (CL~ 30 reticulum) L% HPMC 0.4%

XIV, tegula rubigo signaculi ceramici formulae

Formulae I;Redispersible polymer pulveris RDP 1.5 ~ 2%, ordinaria caementa Portlandiae 30%, alumina alta caementum 10%, vicus harenae 30%;duplex musca pulveris XXVIII% HPMC 0.4%

Formulae duae;Redispersible polymer pulveris RDP 3~5%, ordinarium caementum Portlandiae 25%, alumina alta caementum 10%, vicus arena 30%;duplex muscapulveris XXVI%, pigmento V% HPMC 0.4%

XV, arida pulveris IMPERVIUS efficiens formulae

IMPERVIUS coatingRedispersible polymer pulveris RDP 0,7~1%, caementum (caementum nigrum) 35%, calcii grisei pulveris 20%, vicus arenae (tenuitatis > 200 reticulum 35%;duplex musca pulveris X% HPMC 0.4%

16, pulveris gypsi tenaces formulae

Formula 1: gypsum tenaces pulveris 0.7 ~ 1.2%, emplastrum Parisiense (gypsi aquae dimidium, gypsi pulveris) 100% HPMC 0.4%

Formulae duae: gypsum tenaces pulveris 0.8 ~ 1.2%, emplastrum Parisiense (gypsi aquae dimidium, gypsi pulveris) 80%;duplex musca pulveris (gravis calcii) 20% HPMC 0.4%

XVII, pingere gypsi pulveris formulae

Formulae una: gesso tectorio pulvere 0.8 ~ 1%, emplastrum Parisiense (gesso aqua dimidia, gesso pulvere) 100%. HPMC 0.4%

FORMULA 2: gesso tectorium pulveris 0.8 ~ 1.2%, emplastrum Parisiense (gesso aquae dimidium, gesso pulveris) 80%, pulvis muscae duplex (gravis calcii) 20% HPMC 0.4%

18. Formulae aquarum substructio lignorum putty pulveris

Aquam - lignum puttyRedispersible polymer pulveris RDP 8~10%;duplex musca pulveris (gravis calcii pulveris) 60%, gypsi pulveris 24%, talci 6~8% HPMC 0.4%

XIX, princeps anhydrite putty pulveris formula

putty gummi pulveris 0,5 ~ 1.5%, emplastri emplastri cocti (aedificare gesso, gesso aquae dimidium) 88%, talc pulveris (vel muscae duplex pulveris) 10%, gesso mora coagulantis 1% HPMC 0.4%

20. Formulae gypsi vulgaris pulveris putty

Latex pulveris 1 ~ 2%, emplastrum emplastri cocti (aedi gesso, gesso aquae dimidium) 70%, talc pulveris (vel muscae duplex pulveris) 30%, gesso mora coagulantis 1% HPMC 0.4%